Surfacing of worn out places at bearings of sliding

Initially, the necessary preparatory operations are performed, the recommended sequence of operations is as follows:

  • On the defective places, the remnants of the old Babbitt are removed with a gas-oxygen cutter;
  • The surface of the liner is cleaned of oxides and scale with the use of rigid metal brushes;
  • The surface is degreased, which is prepared for surfacing, after which it is thoroughly washed with hot water;
  • Tinning of the surface is carried out using fluxes.

Surfacing and subsequent machining of the bearing housing is performed as follows. Set the value of allowance, which is necessary for subsequent processing on machines, after which the surfacing is carried out alternately each of the liners separately. Further, surface slags and oxides are removed, as well as previously supplied process plugs.

Mechanical treatment of welded surfaces

The contact details are placed «on the paint», and, using the feeler gauge, monitor the actual value of the gaps. Installation of tightening bolts is not required. As a result, a possible shift of the bearing halves is established, which should not exceed 0.02 mm. Having convinced in qualitatively executed shabrenija, the loose leaf place in the lathe and there check a detail on probable radial palpation: it should not exceed 0,3… 0,5 mm. Further, the working surface of the insert is pierced to the dimensions indicated in the drawing of the assembly. Supplier Avlob offers to buy babbit at a bargain price. The price is the best in this segment of rental.

Quality control

Visual inspection of the surface is performed. It should have a silvery white color, without yellowness. The presence of pores, shells, as well as foreign surface inclusions is not allowed. The final stage of the test is a kerosene test: the product is placed in a container with kerosene for several hours, then it is removed, carefully wiped with rags, rubbed with chalk joints and placed under load. If after the control period of exposure to chalk marks traces of kerosene are found, the coupling of babbitt with the metal is incomplete, and the product requires re-melting. If all control results are positive, the insert is subjected to final milling with the cutting of the end surfaces.